MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SMAC SMACMOUNT® 1242S Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Suspension for :
  • Aircraft avionics components and subassemblies
  • Missile electronics
  • Vehicular electronics requiring vibration isolation
Advantages :
  • Bushing style mount
  • Countersunk for lowest installed height
  • Can be pre-loaded to vary natural frequency
  • Axial to radial springrate ratio is 1:1

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
Axial/Radial frequency ratio1/1 approx.
Frequency20-40 Hz
Load0.5 - 2.5 kgper damper
 20 N1.25 mm, Compression Curve
 35 N2.4 mm, Compression Curve
 5 N0.25 mm, Compression Curve
Maximum axial deflection3 mm
Metal partsAnodized aluminumpassivated stainless steel
Overall size2.6 x 51.2 x 23 mm
Transmissibility at resonance<6
Weight22 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZSMAC020 / 146136

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.