MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lumicene® mPE M 3410 EP HDPE Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and LLDPE.

Applications: Lumicene® mPE M 2710 EP is recommended for clarity shrink films, food packaging, laminations and multilayer packaging film.

Information provided provided by Total Petrochemicals. Also available in the Americas through the Bayport Polymers joint venture.

Key Words: Outstanding clarity and gloss; excellent bubble stability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccASTM D792
Water Vapor Transmission 13.9 g/m²/day
@Thickness 0.0254 mm
Thickness 25.4 micronsas tested; BUR 2.5
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
High Load Melt Index 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 580 %
@Thickness 0.0254 mm
ASTM D882A
Film Elongation at Break, TD 720 %
@Thickness 0.0254 mm
ASTM D882A
Flexural Modulus 0.600 GPaASTM D 790
Elmendorf Tear Strength MD 165 g
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength TD 500 g
@Thickness 0.0254 mm
ASTM D1922
Dart Drop 150 g/mil
@Thickness 0.0254 mm
ASTM D1709A
Dart Drop Test 150 g1.0 mil; ASTM D 1709
Film Tensile Strength at Break, MD 4900 psi
@Thickness 0.0254 mm
ASTM D882A
Film Tensile Strength at Break, TD 4800 psi
@Thickness 0.0254 mm
ASTM D882A
1% Secant Modulus, MD 31000 psi
@Thickness 0.0254 mm
ASTM D882A
1% Secant Modulus, TD 25000 psi
@Thickness 0.0254 mm
ASTM D882A
 
Thermal PropertiesOriginal ValueComments
Melting Point 121 °CASTM D3417
 
Descriptive Properties
ProcessFilm

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene
Baystar™ Lumicene® mPE M 3410 EP Metallocene Medium Density Polyethylene Film Resin
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade)
Dow HDPE 30460M High Density Polyethylene

PFINAP084a / 172237

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.