MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Extramet EMT 609 Tungsten Carbide, Ultra-Fine Grain
Categories: Ceramic; Carbide

Material Notes: EMT 609 is an ultrafine grade used for milling hardened steel (>50HRC). It is ideal for High Speed Cutting (HSC) for mold construction, wear resistant microtools, finish spot milling/secondary chatter reduction and uncoated machining of new composite materials.

Extramet EMT 609 is a homogenous mixture of tungsten carbide grains in a tough cobalt binder matrix. The carbide grains are fused into a solid matrix of cobalt metals. The metal carbide’s grains are “cemented” in the binder metal’s matrix.

Information provided by Extramet

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.3 - 14.5 g/ccISO 3369
Porosity <= 0.00 %B, Particular; ISO 4505
 <= 0.00 %C-Porosity; ISO 4505
 <= 1.0 %A, Basic; ISO 4505
Grain Size 0.50 µmAverage
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1900 - 2000ISO 3878
Modulus of Rupture >= 4.00 GPaTransverse Rupture Strength
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 9.0 %Metals Basis
Tungsten, W 89.5 %Metals Basis
 
Descriptive Properties
Coercive Field Strength32.5-39.5 kA-M-1
Coercive Force 4no13.4-16.4 µT-m3-kg-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Extramet EMT 409 Tungsten Carbide, Fine Grain
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite
Mi-Tech Metals CW80 80 Tungsten/20 Copper PM Metal Composite
Poco Graphite EDM-4 EDM Graphite
Sandvik MP 40 Cemented Carbide Grade for Rotary Tools

EEMT005 / 187008

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.