MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Conventus Polymers Duramide™ 6XMG35 Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Duramide 6XMG35 is a nylon based resin compound with a proprietary combination of fillers designed for structural performance, improved surface appearance, dimensional stability, and UV stability. Available in colors.

Information provided by Conventus Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.17 mm
0.0050 - 0.0070 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 134 MPa19500 psiASTM D638
Elongation at Break 1.0 - 3.0 %1.0 - 3.0 %ASTM D638
Flexural Modulus 8.27 GPa1200 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
Izod Impact, Unnotched 4.81 - 5.87 J/cm9.00 - 11.0 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C395 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 266 - 277 °C510 - 530 °F
Mold Temperature 93.3 °C200 °F
Drying Temperature 79.4 °C175 °F
Dry Time 4.00 hour4.00 hour
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Vent Depth 0.00127 - 0.00254 cm0.000500 - 0.00100 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
YOUJU New Materials Paryls® PPSU F1150

PCONV900 / 233800

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.