MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characterization: Bayflex XGT-16 Clear is an elastomeric polyurethane system used in the reaction injection molding (RIM) process.

Properties / Applications: Bayflex XGT-16 Clear is an elastomeric polyurethane system used in the reaction injection molding (RIM) process. The formulated system is supplied as two liquid components: Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. Bayflex XGT-16 Clear system has a flexural modulus of 16,00 psi* at room temperature. It is used in applications requiring excellent impact properties, such as bumpers for buses and other vehicles. As with any product, use of the Bayflex XGT-16 Clear system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPolyol (Component B)
 1.21 g/ccIsocyanate (Component A)
Density 1.04 g/ccASTM D792
Viscosity 600 cPPolyol (Component B)
 700 cPIsocyanate (Component A)
Thickness 125 mil
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cmBayer Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Hardness, Shore D 45ASTM D2240
Tensile Strength, Ultimate 17.0 MPaASTM D412
Elongation at Break 250 %ASTM D412
Flexural Modulus 0.110 GPaASTM D790
Tear Strength 80.0 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 200H-18 wheel, 1000 g Load; ASTM D3489
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Flash Point 114 °CPolyol (Component B)
 213 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 60.0 - 70.0 °C
Cure Time 2.00 - 3.00 min
 
Descriptive Properties
AppearanceLight yellow to yellow liquidIsocyanate (Component A)
 Yellow or blue-green to amber liquidPolyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PB2B89 / 26631

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.