MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ITW Devcon® Wear Guard™ Ultra Wear-Resistant Epoxy Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Alumina ceramic bead-filled epoxy system with outstanding abrasion resistance for severe service conditions. Use; Repair scrubbers, ash handling systems, pipe elbows, screens and ceramic lined chutes; recontour chippers, bins, hoppers, bunkers, separators; protect exhausters, chutes, launders, housing fans, crushers and breakers. Features: Extends Equipment Operating Cycles, Epoxy Primer FC included (For use as primer), Non-sagging, Outstanding Wear Resistance.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.50 g/cc2.50 g/ccCured
Solids Content 100 %100 %Uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787
Tensile Strength 29.4 MPa4260 psi
Flexural Strength 60.23 MPa8735 psi
Compressive Strength 95.91 MPa13910 psi
Adhesive Bond Strength 10.79 MPa1565 psiLap Shear; w/o beads
Taber Abrasion, mg/1000 Cycles 0.0650.065Weight loss (grams). w/o beads
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hourFunctional cure
Pot Life 20.0 min
@Temperature 23.9 °C
20.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Chemical/Solvent ResistanceSodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayuncured
Coverage44 sq.in/lbCured @ 1/4"
Mix Ratio by weightR:18.8/H:7.8/Beads:73.4
Recoat Time1 to 2 hrs
ViscosityNon-sag putty Mixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9176 / 239686

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.