MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group EP AOSR EPI Engineered Polymers Acrylic Oligomer
Categories: Polymer; Thermoset

Material Notes: EP AOSR, is an aliphatic triacrylate oligomer and is "Powered by Reactamine ®Technology”. EP AOSR is light in color and has fast cure response to UV and EB. EP AOSR exhibits good flexibility, toughness, abrasion resistance, water resistance, and excellent non-yellowing properties.

EP AOSR when used in unsaturated polyesters, allows the styrene monomer content to be reduced to lower V.O.C.’s. Impact strength in gel coats improves, UV stability improves, water resistance increases, and gloss retention is higher. Laminating resin improve in cure and Barcol hardness.

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 9.10 lb/ft³
Solids Content 100 %Polymer Solid
Viscosity 450 cP
@Temperature 25.0 °C
Molecular Weight 1500 g/mol
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
ChevronTexaco Delo® 1000 Marine Engine Oil, SAE 40
ChevronTexaco Cleartex® CF F
Carlisle 201LD Carbon-Carbon Composite

PACC080 / 22207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.