MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® RG-10150 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-10100 series is a group of high performance thermoplastic elastomers specifically designed for regulated applications including food contact, toys, and children’s products. This grade is suitable for injection molding. Monprene RG-10150 is a low density, medium hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Latin America; North America

Features: BPA Free; Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Low Density; Low Flow; Low Specific Gravity; Medium Hardness; Lubricated; No Animal Derived Components; Slip; Without Fillers

Uses: Closures; Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Handles; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Viscosity 226 cP
@Shear Rate 206 1/s,
Temperature 200 °C
226 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50
@Time 5.00 sec
50
@Time 0.00139 hour
ISO 868
Tensile Strength at Break 6.80 MPa986 psiAcross Flow; ISO 37
Tensile Stress at Strain 0.869 MPa
@Strain 100 %
126 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 840 %840 %Across Flow; ISO 37
Tear Strength 11.0 kN/m63.0 pliAcross Flow, Method Ba, Angle (Unnicked); ISO 34-1
 19.3 kN/m110 pliFlow, Method Ba, Angle (Unnicked); ISO 34-1
Compression Set 25 %
@Temperature 70.0 °C,
Time 79200 sec
25 %
@Temperature 158 °F,
Time 22.0 hour
Type A; ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 350 °F
Middle Barrel Temperature 182 - 204 °C360 - 400 °F
Front Barrel Temperature 193 - 216 °C380 - 420 °F
Nozzle Temperature 182 - 227 °C360 - 440 °F
Melt Temperature 182 - 227 °C360 - 440 °F
Mold Temperature 26.7 - 48.9 °C80.0 - 120 °F
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 1.27 cm0.150 - 0.500 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® IN-19147 Thermoplastic Elastomer

PTEKNQ0920 / 237411

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.