MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Hostalen 5231H High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Outstanding balance of stiffness, toughness and environmental stress cracking resistance make Hostalen 5231H the choice of customers for the production of closures for water, CSD and many other types of food and non-food caps and closures. Applications: Caps & Closures, Collapsible Tubes

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ISO 1183-1
Environmental Stress Crack Resistance >= 35 hour
@Temperature 50.0 °C
>= 35 hour
@Temperature 122 °F
cap test, 4Mpa, 2% Arkopal; LYB Method
Melt Flow  2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 5.6 g/10 min
@Load 5.00 kg,
Temperature 190 °C
5.6 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ISO 868
Ball Indentation Hardness 50.0 MPa7250 psiISO 2039-1
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1,-2
Elongation at Yield 10 %10 %ISO 527-1,-2
Tensile Modulus 1.10 GPa160 ksiISO 527-1,-2
Charpy Impact, Notched  0.530 J/cm²
@Temperature -30.0 °C
2.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.04 J/cm²
@Temperature 23.0 °C
4.95 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 74.0 °C165 °FB50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding, compression molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon H 5057 High Denisty Polyethylene
Dow DOWLEX™ IP-10 High Density Polyethylene
LyondellBasell Purell ACP 6541A High Density Polyethylene (HDPE), Injection Molded
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin
Braskem HD7255LS-L HDPE Injection Molding Polyethylene

PEQT8445 / 220080

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.