MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Eccobond® 276 Two-Component Thermally Conductive Epoxy Adhesive and Sealant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Emerson & Cuming 276 Eccobond® Two-Component Thermally Conductive Epoxy Adhesive and Sealant
Highly filled, high temperature resistant, thermally conductive, epoxy adhesive and sealant. Requires heat cure. Excellent chemical resistance. Used for bonding metal, glass and ceramic substrates. Mix ratio = 100:10 (cat 17 M 1). Cure Type: Heat Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.35 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 2700 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 200 °C
 6.00 hour
@Temperature 150 °C
 8.00 hour
@Temperature 120 °C
 
Descriptive Properties
ColorBlack
ViscosityThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg E550 EPDM Rubber
Trelleborg Sealing Solutions HiMod® 924 Thermoplastic Bearing
Trelleborg Emerson & Cuming Eccobond® 285 Two-Component Thermally Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 281 One-Component Thermally Conductive Epoxy Adhesive
Trelleborg E849 EPDM Rubber

PEMERS60 / 35752

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.