MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5383-H321/H116
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Mechanical property data provided by Hoogovens Aluminium Walzprodukte.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95383; AA5383-H321/H116, Aluminium 5383-H321/H116; Aluminium 5383-H116; Al5383-H321/H116
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 305 MPa44200 psi
Tensile Strength, Yield 220 MPa31900 psi
Elongation at Break 10 %10 %
Tensile Modulus 70.3 GPa10200 ksiAluminum 5083
Poissons Ratio 0.330.33Aluminum 5083
Shear Modulus 26.4 GPa3830 ksiAluminum 5083
Shear Strength 184 MPa26700 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000560 ohm-cm0.00000560 ohm-cmAluminum 5083
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
Aluminum 5083
 25.8 µm/m-°C
@Temperature 20.0 - 300 °C
14.3 µin/in-°F
@Temperature 68.0 - 572 °F
average; Aluminum 5083
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F(Aluminum 5083)
Thermal Conductivity 117 W/m-K812 BTU-in/hr-ft²-°F(Aluminum 5083)
Melting Point 585 - 641 °C1090 - 1190 °FAluminum 5083
Solidus 585 °C1090 °F(Aluminum 5083)
Liquidus 641 °C1190 °F(Aluminum 5083)
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.9 - 95.3 %91.9 - 95.3 %As remainder
Chromium, Cr <= 0.25 %<= 0.25 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe <= 0.25 %<= 0.25 %
Magnesium, Mg 4.0 - 5.2 %4.0 - 5.2 %
Manganese, Mn 0.70 - 1.0 %0.70 - 1.0 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.40 %<= 0.40 %
Zirconium, Zr <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
5283 Aluminum Composition Spec
Aluminum 5356
Aluminum 5083-H116; 5083-H321
Aluminum 5182-H34
Aluminum 5252-O

MA5383H321 / 9263

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.