MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crosspolimeri FRAGOM PR/0500 Flame Retardant Halogen Free Polyolefine
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefin thermoplastic compounds.

FRAGOM PR/0500: flame retardant polyolefin thermoplastic compound having high temperature index and good oxygen index, suitable for flexible cable sheathing. The material is heavy-metal and plasticizer free (no migration risks). Suitable to pass more than 30.000 cycles

Certify: EN 50363-8(2005) TM7, CEI 2011 M1

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D792
Melt Flow 10 - 19 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 - 19 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Hardness, Shore D 3737ASTM D2240
Tensile Strength >= 8.00 MPa>= 1160 psiIEC 60811
 >= 9.60 MPa
@Temperature 80.0 °C,
Time 605000 sec
>= 1390 psi
@Temperature 176 °F,
Time 168 hour
Heat Ageing; IEC 60811
Elongation at Break >= 170 %>= 170 %IEC 60811
 >= 204 %
@Temperature 80.0 °C,
Time 605000 sec
>= 204 %
@Temperature 176 °F,
Time 168 hour
Heat Ageing; IEC 60811
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 29 %29 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 110 °C230 °F
Zone 2 120 °C248 °F
Zone 3 140 °C284 °F
Zone 4 160 °C320 °F
Die Temperature 170 - 190 °C338 - 374 °F
Head Temperature 170 °C338 °F
Dry Time  2.00 hour
@Temperature 80.0 °C
2.00 hour
@Temperature 176 °F
 3.00 hour
@Temperature 90.0 °C
3.00 hour
@Temperature 194 °F
 
Descriptive Properties
Halogen Content< 0,2%IEC 60754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS082 / 294166

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.