MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Sulfur bearing Copper, UNS C14700, OS050 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.050 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Butt Weld, Capacity for Being Cold Worked

Common Fabrication Processes: Cold working; Drawing; Extruding; Forging; Hot working; Machining; Rolling; Swaging

Typical uses: Electrical Connectors; Motor Components; Switch Components; Terminal Connectors; Fasteners; Rivets; Screws; Cold Forgings; Cold Headed Parts; Furnace Brazed Articles; Machined Parts; Screw Machine Products; Soldering Coppers; Welding Torch Tips; Plumbing Fittings;

Applicable Specifications: ASTM B224; Bar – Forgings ASTM B124/B124M, ASTM B301/B301M; Brazing Filler Metal – FEDERAL QQ-B-650; Die – Forgings ASTM B283/B283M; Fitting – ASME B16.22; Forgings, Die (Hot Pressed) – ASME SB283; Rod – ASTM B301/B301M, SAE J463, Forgings ASTM B124/B124M, SAE J461; Shapes – ASTM B301/B301M, Forgings ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 40
@Thickness 12.7 mm
Tensile Strength 32.0 ksi
@Thickness 12.7 mm
Tensile Strength, Yield 10.0 ksi
@Thickness 12.7 mm
0.5% Ext
Elongation at Break 52 %
@Thickness 12.7 mm
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 85 %
Forgeability 65 %
Shear Strength 22.0 ksi
@Thickness 12.7 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000181 ohm-cm95% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µin/in-°F
@Temperature 20.0 - 100 °C
 9.60 µin/in-°F
@Temperature 20.0 - 200 °C
 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Thermal Conductivity 216 BTU-in/hr-ft²-°F
Melting Point 1953 - 1969 °F
Solidus 1953 °F
Liquidus 1969 °F
Annealing Point 800 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1400 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.9 %
Phosphorus, P 0.0020 - 0.0050 %
Sulfur, S 0.20 - 0.50 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC14700x4 / 292785

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.