MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical Lutex 810 SBR Latex  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Description: Blister Resistance, Ink set off, Sheet Gloss, Coater Runnability

Application: Art Paper, Web Offset, Blade Coater and Adhesive coated paper

CSA No. 70857-13-5 and 7732-18-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 - 1.05 g/ccLSY-QB-ID002
Solids Content 49.5 - 50.5 %
@Temperature 130 °C,
Time 1800 sec
Dry residual gravimetric; LSY-QB-ID001
Particle Size 115 - 135 µmLaser Light Scattering Method; LSY-QB-ID016
pH 7.5 - 8.5LSY-XB-YD006
Viscosity <= 200 cP
@Time 60.0 sec
#60 spindle, 60 rpm; LSY-QB-ID006
Surface Tension 40 - 50 dynes/cmRing Type; LSY-QB-ID005

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUTEX 820GE Synthetic Latex
LG Chemical LUTEX 5310 Synthetic Latex
Dow Latex LXC 807NA Modified Acrylic Polymer Latex

PLAY234 / 148244

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.