MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid
Categories: Fluid

Material Notes: Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-heat recovery systems.

Applications

  • Gas processing
  • Liquid terminal tank heating
  • Asphalt plants
  • Plastic production

Information Provided by Paratherm Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 42.0 lb/ft³
@Temperature 316 °C
 44.0 lb/ft³
@Temperature 260 °C
 47.0 lb/ft³
@Temperature 204 °C
 49.0 lb/ft³
@Temperature 149 °C
 52.0 lb/ft³
@Temperature 93.3 °C
 54.0 lb/ft³
@Temperature 37.8 °C
 56.0 lb/ft³
@Temperature -17.8 °C
Viscosity 0.48 cP
@Temperature 249 °C
 0.53 cP
@Temperature 238 °C
 0.58 cP
@Temperature 227 °C
 0.63 cP
@Temperature 216 °C
 0.71 cP
@Temperature 204 °C
 0.80 cP
@Temperature 193 °C
 0.89 cP
@Temperature 182 °C
 1.0 cP
@Temperature 171 °C
 1.1 cP
@Temperature 160 °C
 1.3 cP
@Temperature 149 °C
 1.5 cP
@Temperature 138 °C
 1.8 cP
@Temperature 127 °C
 2.2 cP
@Temperature 116 °C
 2.6 cP
@Temperature 104 °C
 3.2 cP
@Temperature 93.3 °C
 4.2 cP
@Temperature 82.2 °C
 5.7 cP
@Temperature 71.1 °C
 7.8 cP
@Temperature 60.0 °C
 12 cP
@Temperature 48.9 °C
 18 cP
@Temperature 37.8 °C
 30 cP
@Temperature 26.7 °C
 54 cP
@Temperature 15.6 °C
 106 cP
@Temperature 4.44 °C
 254 cP
@Temperature -6.67 °C
 720 cP
@Temperature -17.8 °C
Molecular Weight 330 g/molAverage
Vapor Pressure 0.00896 bar
@Temperature 171 °C
 0.0200 bar
@Temperature 193 °C
 0.0393 bar
@Temperature 216 °C
 0.0758 bar
@Temperature 238 °C
 0.131 bar
@Temperature 260 °C
 0.221 bar
@Temperature 282 °C
 0.365 bar
@Temperature 304 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µin/in-°Fconverted from volume expansion
Specific Heat Capacity 0.430 BTU/lb-°F
@Temperature -17.8 °C
 0.480 BTU/lb-°F
@Temperature 37.8 °C
 0.520 BTU/lb-°F
@Temperature 93.3 °C
 0.560 BTU/lb-°F
@Temperature 149 °C
 0.610 BTU/lb-°F
@Temperature 204 °C
 0.650 BTU/lb-°F
@Temperature 260 °C
 0.690 BTU/lb-°F
@Temperature 316 °C
Thermal Conductivity 0.612 BTU-in/hr-ft²-°F
@Temperature 316 °C
 0.672 BTU-in/hr-ft²-°F
@Temperature 260 °C
 0.720 BTU-in/hr-ft²-°F
@Temperature 204 °C
 0.780 BTU-in/hr-ft²-°F
@Temperature 149 °C
 0.828 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 0.888 BTU-in/hr-ft²-°F
@Temperature 37.8 °C
 0.936 BTU-in/hr-ft²-°F
@Temperature -17.8 °C
Maximum Service Temperature, Air 550 °FFired Heaters
 575 °FAll Others
 600 °FFilm Temperature
Minimum Service Temperature, Air 18.0 °Fstart-up temp at 300 cPs
 95.0 °Foperating temp at 20 cPs
Pour Point <= -30.0 °FD97
Flash Point >= 340 °FClosed Cup (D93)
 >= 360 °FOpen Cup (D92)
 
Descriptive Properties
AppearanceClear Amber Colored
BaseAlkylated Aromatic
OdorSweet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WPAR05 / 104383

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.