MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled

Material Notes: TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include:
  • High surface luminosity
  • Easy processability
  • Dimensional stability
  • Insulation
  • Low weight
  • High toughness
  • Low moisture absorption
  • High chemical resistance
Glass fiber reinforced TISAKRIL increases mechanical resistance, surface hardness, melting point and specific gravity, while simultaneously reducing mold shrinkage. Calcite, talc, glass ball and other fillers may be used for reinforcement of TISAKRIL apart from glass fiber. It has excellent chemical resistance to weak acids, weak alkalis, and strong alkalis. It has good resistance against strong acids. It has weak chemical resistance against organic solvents, alcohols, hydrocarbons, and engine fuels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Moisture Absorption 0.20 %ISO 62
Linear Mold Shrinkage 0.0020 cm/cm
Ash 15 %ISO 3451
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 69.0 MPaISO 527-2
Tensile Strength, Yield 70.0 MPaISO 527-2
Elongation at Break 4.8 %ISO 527-2
Elongation at Yield 5.0 %ISO 527-2
Modulus of Elasticity 4.50 GPaISO 527-2
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 575 VTS EN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °C
Vicat Softening Point 108 °CISO 306
Heat Distortion Temperature 110 °CISO 75-2
Flammability, UL94 HB
Glow Wire Test 650 °C60695-2-10
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 °C
Rear Barrel Temperature 190 - 210 °CAft-1. Region Temperature
Middle Barrel Temperature 190 - 210 °CMid-2. Region Temperature
Front Barrel Temperature 190 - 210 °CPre-3. Region Temperature
Nozzle Temperature 200 °C
Melt Temperature 160 - 180 °C
Drying Temperature 80.0 °CPredrying Temperature
Dry Time 2 - 3 hourPredrying Time
 
Descriptive Properties
Block Temperature45°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Absolac® 30GF15 ABS, 15% Glass Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Cheng Yu Plastic A702G15 ABS 15% Glass Fiber Reinforced
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced

PTIS061 / 79496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.