MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox HMa Methyl isobutyl ketone peroxide
Categories: Other Engineering Material

Material Notes: Trigonox HMa is a methyl isobutyl ketone peroxide (MIBKP) formulation for curing unsaturated polyester resins as such or in the presence of a cobalt accelerator in the temperature range of 60-150°C.

CAS number: 37206-20-5

EINECS/ELINCS No: 253-396-4

Applications: Trigonox HMa is a methyl isobutyl ketone peroxide (MIBKP) formulation for the curing of unsaturated polyester resins as such or in the presence of a cobalt accelerator in the temperature range of 60-150°C. Trigonox HMa can be used in combination with a cobalt accelerator (e.g. Accelerator NL-49PN) for those applications where a long gel time or production time is required at ambient temperature and a fast cure at higher temperatures e.g. 60-100°C. Application area can be: filament winding and production of flat and corrugated sheets. Trigonox HMa shows also without the addition of a cobalt accelerator a high reactivity at elevated temperatures, which is demonstrated by its low activation temperature. Trigonox HMa can therefore successfully be used in the temperature range of approximately 80-150°C: for the production of flat and corrugated sheets where a discoloration by the cobalt accelerator is not acceptable, as kicker for the pultrusion application in combination with a low reactive peroxide like Trigonox 29-IN50 or Trigonox C. The low reactive peroxide must be included in the formulation in order to achieve a complete cure.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
Viscosity 12 cP
@Temperature 20.0 °C
12 cP
@Temperature 68.0 °F
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 55.0 °C131 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearanceClear liquid
Color=50 Pt-Co
Content10.0-10.3 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1196 / 286719

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.