MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MetalTek MTEK SD100 Cast UNS J93380 Duplex Stainless Steel
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel; Cast Stainless Steel

Material Notes: Information provided by MetalTek

Key Words: Cast Grade CD3MWCuN, 6A; Cast ASTM A890, ASTM A995; Wrought Grade ZERONĀ® 100
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 235
Tensile Strength, Ultimate >= 690 MPa
Tensile Strength, Yield >= 450 MPa
Elongation at Break >= 25 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 22.5 - 25.5 %
Copper, Cu 0.50 - 1.0 %
Iron, Fe 55.17 - 65.30 %As Balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo 3.0 - 4.0 %
Nickel, Ni 8.0 - 11 %
Nitrogen, N 0.20 - 0.30 %
Silicon, Si <= 1.0 %
Tungsten, W 0.50 - 1.0 %
 
Descriptive Properties
Heat TreatmentSol. Anneal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 4501 Duplex Stainless Steel
MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel
MetalTek MTEK 29MN Cast UNS J93372 Duplex Stainless Steel
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel
Sandvik SANMAC SAF 2205 Bar Steel

NMETEK063x / 140958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.