MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Saint-Gobain Versilon™ R-3400 UV Resistant Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Tygon® R-3400: Ideal for virtually any permanent or temporary chemical transfer application, Tygon® UV Resistant Tubing combines suppleness and flexibility with resistance to a wide range of chemicals. It shows exceptional resistance to strong acids and many alkalies. The flexibility of Tygon® UV Resistant Tubing makes it quick and easy to put into service, providing considerable savings on installation time and cost. Black in color, it is resistant to ultraviolet light, ozone and weathering, making it ideal for many outdoor applications. Standard sizes of Tygon® UV Resistant Tubing have sufficient wall thickness to block transmission of all UV light. Additionally, in-house testing indicates a UL 94V-O and UL 94HB flammability rating.

Features/Benefits:

    Black in color; Protects light sensitive fluids
  • Wide range of chemical resistance
  • Ozone resistant
  • Excellent burn resistance
  • Low compression set; Resists permanent deformation
  • Available in clear formulation for fluid flow monitoring
Typical applications include Acid and Caustic Transfer, Corrosive Diffusible Gases, Fertilizer and Pesticide Dispensing, Electrical Insulation Lines, Ink and Adhesive Dispensing, General Maintenance
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792-91
Water Absorption 0.19 %24 hours at 23°C; ASTM D570-95
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6415 seconds; ASTM D2240-97
Tensile Strength, Yield 2250 psiASTM D412-97
Elongation at Break 350 %ASTM D412-97
100% Modulus 1.00 ksi
@Strain 100 %
ASTM D412-97
Tear Strength 185 pliInitial Tear Strength; ASTM D1004-94
Compression Set 64 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 56 %ASTM D412-97
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 490 V/milASTM D149-95
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Brittleness Temperature -6.00 °FASTM D746-95
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTGQZ198 / 68712

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.