MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chemours Zonyl™ MP 1000 PTFE Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Zonyl™ MP 1000 fluoroadditive is a white, free-flowing, PTFE powder designed for use as an additive in other materials or as a dry lubricant. It can be used at temperatures from –190 °C to 250 °C (–310 °F to 480 °F), and is inert to nearly all industrial chemicals and solvents. It is a good electrical insulator, does not absorb water, and is highly resistant to weathering. Features: Low surface energy, improved lubricity and wear in plastics and elastomers, and improved performance in lubricants under severe conditions. Applications: Typical loadings of 5 to 20% by weight are used. Plastics that can benefit in this manner include polyacetals, polyamides, polycarbonates, polyesters, polyimides, polysulfides, and polysulfones; elastomers include acrylates, fluoroelastomers, neoprenes, nitriles, and silicones. Added to high-viscosity specialty lubricants designed for use under high pressure, Zonyl™ MP 1000 may increase lubricity and service life, especially at high temperatures or in corrosive environments. It has been used in silicone, fluorosilicone, and hydrocarbon lubricant bases. Smooth, uniform suspensions can be made using conventional blending methods.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³ASTM D4894
Specific Surface Area 5.0 - 10 m²/g5.0 - 10 m²/gASTM D4567
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -190 °C-310 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8852 / 268779

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.