MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Lucite® 47 Glass Separation Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Improper storage and transport of glass products (e.g. flat glass or fabricated items) can lead to costly damage caused by glass-to-glass abrasion and/or corrosion rendering it unsuitable for end-use. Lucite® Acrylic Resins in combination with adipic acid provides excellent protection of glass during storage and shipment.

The blend of adipic acid with Lucite® acrylic resins provides the following benefits: Prevents glass-to-glass abrasion/scratching; Prevents glass corrosion when blended with adipic acid; Physical separator to ease glass handling; Highly resilient; Inert, non-hazardous; Cost effective; Perfectly suited for automated glass handling/processing; Easy to apply; Easy to remove

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.30 %0.30 %
Particle Size 130 - 170 µm130 - 170 µm
Viscosity Measurement 0.40 - 0.600.40 - 0.60Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595
Tensile Strength 73.0 MPa10600 psi
Elongation at Break 4.0 %4.0 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4911.491
Transmission, Visible 92 %92 %
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUCIT9494 / 150208

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.