MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ITW Devcon® Tru-Bond™ LOCA 5000 Coating
Categories: Polymer; Thermoset

Material Notes: Devcon® Tru-Bond™ LOCA products are high clarity, fast curing, UV light curing products. They are engineered to eliminate the air gap between the cover lens of touch panels and display devices. These liquid dispensed, ultra-low hardness products help reduce stresses that contribute to Mura while helping to increase the impact resistance and durability of the assembly.

Cure as tested: LED 365 lamp, illumination intensity= 150mV/cm², total energy 1500 mJ/cm²

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccuncured
 0.990 g/cc0.990 g/cccured
Brookfield Viscosity 5000 cP5000 cPBrookfield RV Spindle 4, 10 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535ASTM D2240
Tensile Strength 0.100 MPa14.5 psiASTM D638
Elongation at Break 600 %600 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.5
@Frequency 1e+6 Hz
5.5
@Frequency 1e+6 Hz
cured.
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -61.0 °C-77.8 °Fcured
Shrinkage 2.33 %2.33 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.461.46cured
Haze <= 0.40 %<= 0.40 %After 500 cycles @ -40°C (30min) to 85°C (30min); ASTM D1003
 <= 0.40 %<= 0.40 %After 500 hours @ 85°C; ASTM D1003
 <= 0.40 %<= 0.40 %After 500 hours @ 85°C/85% RH; ASTM D1003
 <= 0.40 %<= 0.40 %After 500 hours exposure to 0.89 W/m² UV light @ 50°C; ASTM D1003
 <= 0.40 %
@Thickness 0.100 mm
<= 0.40 %
@Thickness 0.00394 in
0.1 mm thick layer adhesive between 2 pcs 1 mm thick panel glass; ASTM D1003
Transmission, Visible  >= 99.5 %
@Wavelength 550 nm
>= 99.5 %
@Wavelength 550 nm
0.1 mm thick layer adhesive between 2 pcs 1 mm thick panel glass; ASTM D1003
 >= 99.5 %
@Wavelength 550 nm
>= 99.5 %
@Wavelength 550 nm
After 500 cycles @ -40°C (30 min) to 85°C (30 min); ASTM D1003
 >= 99.5 %
@Wavelength 550 nm
>= 99.5 %
@Wavelength 550 nm
After 500 hours @ 85°C; ASTM D1003
 >= 99.5 %
@Wavelength 550 nm
>= 99.5 %
@Wavelength 550 nm
After 500 hours @ 85°C/85% RH; ASTM D1003
 >= 99.5 %
@Wavelength 550 nm
>= 99.5 %
@Wavelength 550 nm
After 500 hours exposure to 0.89 W/m² UV light @ 50°C; ASTM D1003
 
Descriptive Properties
ColorClear liquidUncured
Storage Modulus (kPa)12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9224 / 239733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.