Key Features:- Excellent thermal conductivity
- Fast curing
- Withstands thermal cycling and shock
- Serviceable from 100°F to +400°F
Product Description: Master Bond Supreme 3HTND 2GT is a fast curing, toughened multifunctional one component high performance epoxy system that can be used for bonding, sealing, glob top and die attach applications. It has a huge array of highly desirable features, including no mixing, a convenient viscosity, sterling physical properties and very fast cures. Unlike many epoxies it can be readily and efficiently applied to a defined area. This epoxy combines excellent electrical insulation properties and thermal conductivity with top-notch dimensional stability and the capability of withstanding rigorous thermal cycling and shocks. It cures in 20-30 minutes at 250°F or in 5-10 minutes at 300°F with very low shrinkage. Supreme 3HTND-2GT can cure in thicknesses of up to 1/8 inch if needed. It bonds well to a wide variety of substrates used in electronics, including metals, composites, ceramics and many plastics. The service temperature range for this system is first rate at -100°F to +400°F. It resists chemicals rather well, including water, acids, bases and many solvents. Especially noteworthy, is its low level of ionic impurities. Supreme 3HTND-2GT is yellowish tan in color. As mentioned above, this multifaceted system can be used as a glob top or die attach and in other applications as an adhesive or sealant in electronics when the special combination of properties, particularly the limited flow characteristics when curing are desirable. Product Advantages: - Single component system; no mixing needed prior to use
- Convenient handling; ideal flow for die attach and glob top applications
- 100% reactive, no volatiles emitted during cure
- Outstanding electrical insulation properties and thermal conductivity
- Excellent physical strength properties
- Sterling dimensional stability
- Service temperature range of -100°F to +400°F
- Offers exquisite protection to electronic components
- Available and easily dispensed from syringes
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |