MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt NORSODYNE® FIREBLOOK I 81268 F Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated Polyester Resin in styrene filled, without halogeneous component and antimony trioxide

Appearance: White

Main resin characteristics: With fillers

Main applications: General purpose

Molding information: Injection molding, RTM

Curing cycle: 16 h at 80°C + 2 h at 140°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³
Solids Content 65 - 69 %65 - 69 %MT-CU001C
Brookfield Viscosity 550 - 750 cP550 - 750 cPsp 3 rpm 50; MT-CUT23V
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 25.0 MPa3630 psiISO 527
Elongation at Break 60 %60 %ISO 527
Tensile Modulus 3.479 GPa504.6 ksiISO 527
Flexural Strength 60.0 MPa8700 psiISO 178
Flexural Modulus 3.276 GPa475.1 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °FISO 75 -2A
 
Processing PropertiesMetricEnglishComments
Cure Time 23.0 - 33.0 min
@Temperature 23.0 °C
0.383 - 0.550 hour
@Temperature 73.4 °F
Peak, Reactivity at 23°C + 1,2% Co 1% + 1,5% MEKP50; MT-CU151R
Gel Time 16.0 - 22.0 min
@Temperature 23.0 °C
16.0 - 22.0 min
@Temperature 73.4 °F
Reactivity at 23°C + 1,2% Co 1% + 1,5% MEKP50; MT-CU151R
Shelf Life 4.00 Month4.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm115-145°CMT-CU151R; Reactivity at 23°C + 1,2% Co 1% + 1,5% MEKP50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP

PPOLYN9337 / 231932

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.