MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Henkel Loctite® Stycast® US 5002 Two-Component Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Loctite Stycast US 5002 provides the following product characteristics:
  • Unfilled
  • Non-sag on mixing
  • Tack-free in only 1.5 hours

Cure: Room temperature cure

Application: Potting and Encapsulating

Loctite Stycast US 5002 is formulated for high speed sealing and potting applications.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0377 lb/in³Part B
 1.09 g/cc0.0394 lb/in³Mixed
 1.14 g/cc0.0411 lb/in³Part A
Viscosity 4000 cP4000 cPPart B
 8000 cP8000 cPPart A
 17000 cP
@Time 120 sec
17000 cP
@Time 0.0333 hour
Mixed
 90000 cP
@Time 480 sec
90000 cP
@Time 0.133 hour
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min
@Temperature 25.0 °C
16.0 hour
@Temperature 77.0 °F
Gel Time 20.0 min20.0 min100 gram mass, Gel time is longer (@ 30 minutes) in static gel tubes
Shelf Life 6.00 Month6.00 Monthfrom date of manufacture, stored in cool, dry conditions
 
Descriptive Properties
AppearanceBlackMixed
 BlackPart A
 Off-WhitePart B
Mix Ratio, by Volume1 : 1Part A : Part B
Mix Ratio, by Weight100 : 92Part A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7968 / 255452

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.