MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BiologiQ ESR-PE EcoStarch mLLDPE Blend
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin film

Information provided by BiologiQ

Key Words: TPS, ESR, biopolymer, bioresin, biodegradeable
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Water Vapor Transmission 24.0 - 30.0 g/m²/day
@Temperature 39.0 °C
100% RH
Oxygen Transmission 84.4 - 96.0 cc-mm/m²-24hr-atm0% RH
Melt Flow 0.47 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 605 - 659 %ASTM D882
Film Elongation at Break, TD 632 - 696 %ASTM D882
Elmendorf Tear Strength, MD 360 - 494 g/milASTM D1922
Elmendorf Tear Strength, TD 580 - 724 g/milASTM D1922
Dart Drop 300 - 340 g/milASTM D1709
Heat Seal Strength 1400 g/in40 PSI; 0.5 SEC
Heat Seal Strength Initiation Temperature 130 - 180 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 2.0 - 4.0 %ASTM D1746
 
Processing PropertiesOriginal ValueComments
Moisture Content >= 0.35 %ASTM D6980

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Biomax® TPS 2100
BiologiQ EcoStarch GS270 Thermoplastic Starch
DuPont Biomax® TPS 2501
DuPont Biomax® TPS 2700
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic

PBIOLQ02 / 176020

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.