This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Excellent adhesion to ITO, chemical and environmental resistance. This dielectric has been designed to be used with Phosphor C2080211P2 to produce a white light. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester Substrate: ITO coated polyesterInformation provided by Gwent Electronic Materials Ltd. |