MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
COI Ceramics Nextel™ AS-N610 Oxide Ceramic Matrix Composite, Aluminosilicate
Categories: Ceramic; Ceramic Matrix Composite; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air environments and are primarily used in both Aerospace and Gas Turbine applications.

Ceramic Matrix System: Water Based Sol-Gel Processing, Versatile Matrix Chemistry

Typical Applications for Oxide CMCs: Rotocraft Exhaust Systems, Advanced Thermal, Advanced Combustor

Highest Strength

Information from COI Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.83 g/cc
Porosity 25 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 365 MPa
Tensile Stress at Strain 18.0 ksi
@Strain 0.1 %
 34.0 ksi
@Strain 0.2 %
 49.0 ksi
@Strain 0.3 %
Tensile Modulus 124 GPa
Shear Strength 15.0 MPaShort Beam
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
Maximum Service Temperature, Air 1000 °C
 
Descriptive Properties
Nominal Fiber Volume (%)51

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate
COI Ceramics Nextel™ AS-N650 Oxide Ceramic Matrix Composite, Aluminosilicate
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Silicon Carbide, Reaction-Bonded, SiSiC
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina

CCOIC005 / 122045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.