MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KEP Kepital® ET-20S Acetal Copolymer, Conductive
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes:

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.016 cm/cmt = 3 mm
Melt Flow 11.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 40.0 MPa50 mm/min; ISO 527
Elongation at Break 12 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ISO 527
Flexural Strength 67.0 MPaISO 178
Flexural Modulus 2650 MPaISO 178
Charpy Impact, Notched 4.50 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
KEP Kepital® ET-20A Acetal Copolymer, Conductive
KEP Kepital® F20 Acetal Copolymer
KEP Kepital® F10-03H Acetal Copolymer, High viscosity, High rigidity
KEP Kepital® FA-20 Acetal Copolymer, High Stiffness Conductive
KEP Kepital® F30 Acetal Copolymer

PKEP9913 / 185589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.