A blend of fatty esters. STRUKTOL® V-PETS is a processing aid for polymers which can assist compound processing without significant changes in physical properties. STRUKTOL® V-PETS acts as a dispersing agent for powdered materials and can provide more uniform filler incorporation. It improves filler dispersion and the flow properties and release during processing. FDA Status: 175.105; 176.170; 177.1200; 177.1580; 178.2010 |