System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate (PC)
Material Notes:
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness and flowability realize the thin wall of large-scale business machine chassis.
Information provided by Teijin Chemicals Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.21
g/cc
0.0437
lb/in³
ISO 1183
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
@Thickness 4.00 mm
0.0040
-
0.0060
in/in
@Thickness 0.157 in
Linear Mold Shrinkage, Transverse
0.0040
-
0.0060
cm/cm
@Thickness 4.00 mm
0.0040
-
0.0060
in/in
@Thickness 0.157 in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
46.0
MPa
6670
psi
50mm/min; ISO 527
Tensile Strength, Yield
62.0
MPa
8990
psi
50mm/min; ISO 527
Elongation at Break
50 %
50 %
50mm/min; ISO 527
Elongation at Yield
2.0 %
2.0 %
50mm/min; ISO 527
Tensile Modulus
3.30
GPa
479
ksi
1mm/min; ISO 527
Flexural Strength
94.0
MPa
13600
psi
2mm/min; ISO 178
Flexural Modulus
3.20
GPa
464
ksi
2mm/min; ISO 178
Charpy Impact Unnotched
NB
NB
ISO 179
Charpy Impact, Notched
2.20
J/cm²
10.5
ft-lb/in²
ISO 179
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+16
ohm
1.00e+16
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
CTE, linear
60.0
µm/m-°C
@Temperature 20.0 °C
33.3
µin/in-°F
@Temperature 68.0 °F
ISO 11359
CTE, linear, Transverse to Flow
70.0
µm/m-°C
@Temperature 20.0 °C
38.9
µin/in-°F
@Temperature 68.0 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi)
93.0
°C
199
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
83.0
°C
181
°F
ISO 75
Vicat Softening Point
96.0
°C
205
°F
50°C/hr, 50N; ISO 306
Flammability, UL94
V-1
@Thickness 1.00 mm
V-1
@Thickness 0.0394 in
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
5VB
@Thickness 1.80 mm
5VB
@Thickness 0.0709 in
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy
Teijin Panlite® AM-8030 Polycarbonate + Polyester Alloy
Teijin Panlite® AM-9730FZ Polycarbonate + Polyester Alloy
Teijin Multilon TN-7000F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Teijin Multilon TN-7500 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
PTEIJ52 / 69741
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.