MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

The NanoSteel® Company SHS 9700 GMAW OAW Steel Alloy, Cored Wire
Categories: Metal; Ferrous Metal; Alloy Steel; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Coating Description: SHS 9700 GMAW OAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features exceptional abrasive wear resistance with superior toughness and no high-cost nickel, tungsten and molybdenum in material chemistry.

    Key Performance Characteristics
  • 67 - 70 HRc single and double pass weld deposits
  • Cost effective alternative to complex carbides: iron-based chemistry contains no tungsten, no molybdenum and no nickel
  • Provides exceptional wear resistance lasting significantly longer than most chrome carbide and complex carbide alloys
  • High resistance to abrasion while maintaining high toughness
  • Crystalline microstructure is engineered to submicron (400 nm) size
  • Maintains high hardness after exposure to high temperatures

Application Process: GMAW OAW Weld Overlay for Hardfacing

Information Provided by The NanoSteel Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.36 g/cc0.266 lb/in³Weld Deposit Property
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 67 - 7067 - 70
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 5.0 %<= 5.0 %
Boron, B <= 6.0 %<= 6.0 %
Carbon, C <= 2.0 %<= 2.0 %
Chromium, Cr <= 18 %<= 18 %
Iron, Fe >= 60 %>= 60 %
Manganese, Mn <= 2.0 %<= 2.0 %
Niobium, Nb (Columbium, Cb) <= 5.0 %<= 5.0 %
Silicon, Si <= 2.0 %<= 2.0 %
 
Descriptive Properties
Impact ResistancePassed multiple impacts at 165 ft-lbsDrop Impact Testing
Wear Resistance Mass Loss (g)0.09-0.176000 cycles; ASTM G65-04 Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 50 mm (2 in.) round
AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
AISI 1019 Steel, cold drawn
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

NNANO017 / 106812

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.