MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis RD204CF Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: RD204CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD204CF is recommended for blending, food packaging, high quality stationery, lamination films, and textile packaging film. Additives: RD204CF Free of slip and antiblock and without CaStearate.

Information provided by Borealis AG

Key Words: PP-R
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.910 g/ccbase resin; ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 550 - 750 %ISO 527-3
Film Elongation at Break, TD 550 - 750 %ISO 527-3
Tensile Modulus 500 - 600 MPaMD/TD; ISO 527-3
Flexural Modulus 1000 MPaISO 178
Dart Drop, Total Energy 17.0 J
@Thickness 0.0500 mm
1100N; ISO 7765-2
Coefficient of Friction >= 0.40film/film; ISO 8295
Film Tensile Strength at Break, MD 30.0 - 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 25.0 - 45.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 148 - 154 °CDSC; ISO 3146
Vicat Softening Point 139 °C
@Load 1.02 kg
A50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze <= 2.0 %ASTM D1003
Gloss >= 120 %20° of arc; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis RD208CF Polypropylene Random Copolymer
Borealis RD234CF Polypropylene Random Copolymer
Borealis Bormed™ RD808CF Polypropylene Random Copolymer
Borealis Bormed™ RD804CF Polypropylene Random Copolymer
Borealis RD226CF Polypropylene Random Copolymer

PBOREA569 / 108828

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.