MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek PlatSil® Gel-10 Platinum-cured silicone system
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: PlatSil® Gels are 1A:1B (by weight or volume) platinumcured silicone systems that can be used as mold rubbers, to create prosthetic appliances, and for life casting. Polytek offers an array of accessory products that can be used independently or in concert to increase working time, accelerate cure time, thicken the mix for brushing/layering, thin the mix for easier pouring, or soften or harden the rubber. Smith’s Theatrical Prosthetic Deadener and PlatSil® Deadener LV can be added to soften and eliminate the snappy, synthetic look and feel of ordinary silicone rubbers. “Deadened” PlatSil Gels can be made to look, feel and move like living tissue. Unlike silicone fluid, Deadener does not leach from the cured rubber/appliance, so bonding and use are far easier. PlatSil Gel-OO30 & PlatSil Gel-OO20 are lower in viscosity and are less tacky on cure compared to PlatSil Gel-OO.

Product Line Features:

  • Add “Deadener” to create ultra-realistic prosthetic appliances with varying skin effects and levels of adhesion/tack
  • Add PlatSil Part H Hardener to increase the Shorehardness up to A40
  • Fast-setting options (30-minute demold times) available
  • PlatSil® 71/73 Part R Retarder slows the cure
  • PlatSil® 71/73 Part X Accelerator speeds the cure
  • PlatThix thickens to a brushable mix
  • Bonds to Poly Plastics

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Viscosity 15000 cP15000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1010
 
Processing PropertiesMetricEnglishComments
Cure Time 6.00 min0.100 hourPour Time
 30.0 min0.500 hourDemold Time
 1440 min24.0 hourTotal Cure
 
Descriptive Properties
Cured ColorMilky White
Mix Ratio By Weight1A:1B
Part A ColorMilky White
Part B ColorMilky White
Specific Volume25 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5016 / 251008

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.