MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem PROAID® AC-712 Process Aids
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Proaid AC-712 is a blend of high molecular weight aliphatic fatty acid esters bound to chemically inert fillers designed to act as a processing aid for all natural and synthetic rubber compounds. Proaid AC-712 reduces compound viscosity and improves mold flow (especially transfer and injection) and release from all metal surfaces without affecting cured physical properties.

Applications: The dosage for Proaid AC-712 is 2 to 5 phr, depending on the polymer and the process. Use the higher levels in non-black loaded compounds and in those applications where maximum flow is required. Proaid AC-712 may be used:

  • To improve mold filling and cured part finish
  • To improve flow characteristics in injection and extrusion equip.
  • To improve release from molds, mills and internal mixers
  • To improve dispersion of fillers during mixing (add early in mix)

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Ash 21.5 %
 
Thermal PropertiesOriginal ValueComments
Softening Point 60.0 °C
 
Descriptive Properties
AppearanceWhite pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH355 / 315273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.