Maxxam FR WC 0521-48 is a flame retardant polyolefin compound characterized by low smoke development and good processability. Designed for thin-wall extrusion applications. UL Yellow Card approval for Plenum cable compounds - Component (E203704). Non-halogenated version of Maxxam FR WC0587-21. |