MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CENTROPLAST CENTRODAL TF Polyoxymethylene + PTFE
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: This material is high strength and high heat strength dimensional stability. Applications include racks and annular gears, dimensionally accurate structural components for pumps, and housings and transmission components subjected to high loads.

Information provided by CENTROPLAST Engineering Plastics GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.65 %in water at 23°C; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84
@Thickness 10.0 mm
ISO 2039-2
Ball Indentation Hardness 120 MPavalue at 30 sec.; ISO 2039-1
Tensile Strength, Yield 48.0 MPav = 50 mm/min; ISO 527-2
Elongation at Break 16 %ISO 527-2
Tensile Modulus 2.50 GPaISO 527-2
Flexural Modulus 2.40 GPaISO 178
Charpy Impact Unnotched 6.00 J/cm²ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 100 Hz
IEC 60250
 3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 33.0 kV/mmin transformer oil; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.0080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 °C
ISO 11359
Thermal Conductivity 0.250 W/m-K
Melting Point 166 °C10K/min; ISO 3146
Maximum Service Temperature, Air 105 °CLong Term
 150 °CShort term
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CISO 75-2
Vicat Softening Point 145 °CVST/B/50; ISO 306
Minimum Service Temperature, Air -20.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Compliance
 
Descriptive Properties
Food ComplianceyesBGVV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber
Barlog Plastics KEBAFORM C 2527 POM Copolymer, 25% glass fiber reinforced
Barlog Plastics KEBAFORM C 1090 POM Copolymer, 10% glass fiber reinforced
Azoty Tarnow™ TARNOFORM 500 GF6 POM
Celanese Celcon® LW90F5 Tetrafluoroethylene Filled Acetal Copolymer

PCENTR02 / 27953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.