MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 66H NT0694 Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded

Material Notes: Vydyne 66H NT0694 is a high-viscosity, heat-stabilized PA66 resin with ideal shear-thinning behavior for injection-molding and extrusion applications. It offers a combination of high strength, rigidity, toughness, abrasion resistance, chemical resistance, and thermal stability making it appealing for a broad range of applications. It is available in natural color only.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.5 %2.5 %50% RH; ISO 62
Water Absorption at Saturation 8.5 %8.5 %ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.021 cm/cm
@Thickness 2.00 mm
0.021 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiDry; ISO 527-2
 70.0 MPa10200 psiConditioned; ISO 527-2
Tensile Strength, Yield 55.0 MPa7980 psiConditioned; ISO 527-2
 85.0 MPa12300 psiDry; ISO 527-2
Elongation at Break 40 %40 %Dry; ISO 527-2
 250 %250 %Conditioned; ISO 527-2
Elongation at Yield 5.0 %5.0 %Dry; ISO 527-2
 20 %20 %Conditioned; ISO 527-2
Tensile Modulus 1.90 GPa276 ksiConditioned; ISO 527-2
 2.85 GPa413 ksiDry; ISO 527-2
Flexural Strength 30.0 MPa4350 psiConditioned; ISO 178
 80.0 MPa11600 psiDry; ISO 178
Flexural Modulus 0.900 GPa131 ksiConditioned; ISO 178
 3.00 GPa435 ksiDry; ISO 178
Poissons Ratio 0.400.40Dry; ISO 527-2
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 180
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 180
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 180
 30.0 kJ/m²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 180
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm
@Thickness 0.750 mm
1.00e+14 ohm-cm
@Thickness 0.0295 in
IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 260 °C500 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 80.0 °C68.0 - 176 °FBlow Film Air Temperature
 250 - 295 °C482 - 563 °FCylinder - Extrusion
Die Temperature 270 - 295 °C518 - 563 °FExtrusion
Melt Temperature 270 - 295 °C518 - 563 °FExtrusion
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
FDA YesYes21CFR 177.1500
 
Descriptive Properties
Agency RatingsASTM D 4066 PA0114
 ASTM D 6779 PA0114
 EU 10/2011
 EU 2023/2006
FeaturesGasoline Resistant
 General Purpose
 Good Chemical Resistance
 Good Toughness
 Heat Stabilized
 High Melt Stability
 High Rigidity
 High Strength
 High Viscosity
 Oil Resistant
 Solvent Resistant
Melt Pressure MPa3 to 17
Screw DesignGP or Barrier
UsesAutomotive Applications
 Film
 Monofilaments
 Profiles
 Sheet

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZASCE9759 / 220862

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.