MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ICO Polymers ICOTEX™ 520-5050 500 Micron LDPE Powder
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Masterbatch Grade

Material Notes: Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry.
Key Characteristics: good melt flow and fast and accurate melting.

Information provided by ICO Polymers.

A Schulman acquired ICO, Inc. in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.914 g/ccASTM D1505
Particle Size >= 150 µmpan, 10%
 <= 500 µmsieve < 5%
Melt Index of Compound 22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9.00 MPaASTM D638
Tensile Strength, Yield 9.00 MPa50 mm/min; ASTM D638
Elongation at Break 90 %50 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 °CDSC; ASTM D3418
 140 °Cfusing temperature
Vicat Softening Point 78.0 °CASTM D1525
Brittleness Temperature -45.0 °CASTM D638
 
Descriptive Properties
Max Dry Flowmax 31 sec/100gASTM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 1412 Injection Molding Resin
Chevron Phillips Marlex® 1409 Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Chevron Phillips KN 230 LDPE Injection Molding Resin
Chevron Phillips KN 226B LDPE Injection Molding Resin

PICO037 / 48010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.