MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. MatWeb has other entries for different compounds of this Hypalon grade.

General Hypalon® Information: Vulcanizates of this chlorosulfonated polyethylene synthetic rubber are highly resistant to ozone, oxygen, weather, heat, oil, and chemicals. Hypalon resists discoloration on exposure to light and is widely used in light-colored vulcanizates. It can be compounded to give excellent mechanical properties. Several grades are available, all of which may be processed and used in the usual manner for solid elastomeric vulcanizates. Various grades of Hypalon have been used in single-ply roofing systems; auto power steering and oil cooler hoses; chemical-resistant liners; cable sheathing; and other coatings.

Information provided by DuPont Dow Elastomers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 50
@Temperature 135 °C
ML 1+4.  Stock property.; ASTM D1646-81
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76ASTM D2240-81
Tensile Strength, Ultimate 19.1 MPaASTM D412-80
Elongation at Break 250 %ASTM D412-80
100% Modulus 0.0158 GPa
@Strain 100 %
ASTM D412-80
Compression Set 27 %
@Temperature 100 °C
22 hr at 100°C. Method B. ASTM D395-69.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
DuPont Mobility and Materials Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer
DuPont Mobility and Materials Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
DuPont Mobility and Materials Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound

PDVM05 / 34219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.