MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen HP640U Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Moplen HP640U is a High Flow Polypropylene for Thin Wall Injection Molding. Applications: Clear Containers, Containers, House wares, TWIM Food Containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
Melt Flow 75 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 37.0 MPa
Elongation at Yield 9.0 %
Flexural Modulus 1750 MPa
Izod Impact, Notched 26.0 J/m
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Moplen RP220M Polypropylene Copolymer
BASF Novolen® 3336 MC Polypropylene
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer

PEQT9066 / 220697

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.