MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics SPRING-LINE® Beryllium-Copper Gasket
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Description: SPRING-LINE beryllium-copper gaskets combine high levels of EMI shielding effectiveness with spring-finger wiping and low closure force properties. The high performance qualities of beryllium-copper – high tensile strength, excellent anti-corrosion properties, and good electrical conductivity – make it an ideal material for MEI shielding over a broad frequency range. SPRING-LINE shielding gaskets are available in bright tin, bright copper, and bright copper, and bright nickel finishes, and others upon request. Strips can be soft soldered or resistance welded without damage to their working surface. SPRING-LINE gaskets can be applied by edge mounting using integral clips, or by high tack, pressure-sensitive adhesive.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 2.00 - 6.00 microns0.0787 - 0.236 milGeneral plating (excluding exotic metals)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 38 - 4438 - 44
Tensile Strength >= 1210 MPa>= 175000 psiASTM D412
Tensile Strength, Yield >= 1030 MPa>= 150000 psi
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.8 - 2.0 %1.8 - 2.0 %
Cobalt, Co >= 0.20 %>= 0.20 %plus Nickel
 <= 0.60 %<= 0.60 %plus Nickel plus Iron
Copper, Cu 97.4 - 98 %97.4 - 98 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy 3 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17510)
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze
CMW® ELKALOY D Copper Alloy, Aluminum Bronze
CMW® 73 Copper Alloy

PCHOME273 / 130983

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.