Notes: 66GF6 is a 30% glass fiber reinforced nylon 66 that offers good mechanical performance coupled with good surface finish and flow. Availability: Europe Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight Features: Good Flow; Good Surface Finish Processing Method: Injection Molding Information provided by Teknor Apex |