MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established. - Excellent Adhesion to PC, ABS, PC/ABS, Copolyester - Soft Touch Feel - Water Clarity

Color concentrates with Versaflex™ OM 9-802CL as the carrier are most suitable for coloring this product. If an OM 9-802CL based color concentrate is desired, it is important that the chosen color house have underwater pelletization capabilities. Typical loadings for color concentrates are 1% to 5% by weight. A high color match consistency can be obtained by the use of precolored compounds available from GLS. Polypropylene (PP) based color concentrates are not recommended because they lead to poor dispersion, loss of clarity and can significantly affect adhesion of the TPE to the substrate. Concentrates based on other TPEs should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polystyrene (PS) or polypropylene (PP). Regrind levels up to 20% can be used with Versaflex™ OM 9-802CL with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 300 to 600 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.928 g/ccASTM D792
Viscosity 16000 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
Linear Mold Shrinkage, Flow 0.0040 - 0.011 cm/cmASTM D955
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 100 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4010 sec; ASTM D2240
Tensile Strength at Break 6.41 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 1.59 MPa
@Strain 100 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
 2.14 MPa
@Strain 300 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 1100 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tear Strength 24.5 kN/mASTM D624
Compression Set 20 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B
 99 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 166 - 188 °C
Middle Barrel Temperature 182 - 204 °C
Front Barrel Temperature 193 - 210 °C
Nozzle Temperature 193 - 210 °C
Mold Temperature 21.1 - 26.7 °C
Back Pressure 0.000 - 0.621 MPa
Screw Speed 25 - 75 rpm
 
Compliance PropertiesOriginal ValueComments
FDA YesUnspecified Rating
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGood Colorability
 High Clarity
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesConsumer Applications
 Flexible Grips
 Overmolding
 Soft Touch Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE)
Avient Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE)
Avient Versaflex™ CL2000X Thermoplastic Elastomer (TPE)
Avient Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE)
Avient Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE)

PH0POL0492 / 145061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.