Base Polymer: Polycarbonate Filler/Additive System: special filler, antioxidant Special Features: high light transmission, light scattering, UV stabilized, high flow Market Segment: Automotive, Lighting Application Area: light transparent components Typical Applications: lamp covers, light guides Information provided by Albis Plastics |