MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex TruVis Esters™ TOTM TriOctyl Trimellitate
Categories: Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.989 g/cc0.989 g/cc
Moisture Absorption <= 0.0500 %<= 0.0500 %
Viscosity  9.5 cP
@Temperature 100 °C
9.5 cP
@Temperature 212 °F
 86.5 cP
@Temperature 40.0 °C
86.5 cP
@Temperature 104 °F
Viscosity Measurement 8484Viscosity Index
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10mg KOH/g
 
Thermal PropertiesMetricEnglishComments
Pour Point -35.0 °C-31.0 °F
Flash Point 256 °C493 °F
 
Descriptive Properties
AppearanceClear
Color75Pt/Co Scale
Ester Content (%), min99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Palatinol® TOTM Tri Octyl Trimellitate
The Chemical Company ChemFlexx™ TOTM Trimellitate Plasticizer
LG Chemical TOTM Plasticizer
Geon® Performance Solutions Synplast™ TOTM-N Tri (2-ethylhexyl) Trimellitate
Geon® Performance Solutions Synplast™ TOTM-E Tri (2-ethylhexyl) Trimellitate

PTEKNO829 / 129010

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.