MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 239C Promoted mixture of cumyl hydroperoxide and tert-butyl peroxybenzoate
Categories: Other Engineering Material

Material Notes: Trigonox 239C is a peroxide mixture based on cumyl hydroperoxide, tert-butyl peroxybenzoate and Promotor, especially developed to improve the efficiency curing of vinylester resins in combination with a cobalt accelerator.

CAS number: 80-15-9; 614-45-9

EINECS/ELINCS No: 210-254-7; 210-382-2

Applications: Trigonox 239C is a peroxide mixture based on promoted cumene hydroperoxide and tert-butyl peroxybenzoate. Trigonox 239C is especially developed to improve the cure efficiency of vinylester resins in combination with a cobalt accelerator at elevated temperatures. An application of use can be filament winding. In this application Trigonox 239C can successfully be used instead of generally peroxides like Trigonox 239 and Butanox LPT-IN with the features of no gassing and an improved cure efficiency.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Viscosity 5.0 cP
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Content5%Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1071 / 286594

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.