MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2000 HC A Polyester Alloy Medical Cleaner Resistant - UV Stabilized
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: RTP 2000 HC series are polyester alloys designed to withstand the aggressive cleaners used to disinfect medical equipment

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.2 MPa6700 psiASTM D 638
Elongation at Break >= 100 %>= 100 %ASTM D 638
Tensile Modulus 1.31 GPa190 ksiASTM D 638
Flexural Strength 56.9 MPa8250 psiASTM D 790
Flexural Modulus 1.45 GPa210 ksiASTM D 790
Izod Impact, Notched 8.01 J/cm
@Thickness 3.20 mm
15.0 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C195 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 51.7 - 79.4 °C125 - 175 °F
Drying Temperature 87.8 °C
@Time 14400 - 21600 sec
190 °F
@Time 4.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 103 - 138 MPa15000 - 20000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON MT9140L4 PPS, 40% Medical Technology
Covestro Makroblend® UT305 PC/PET Blend
Covestro Apec® 1803 Polycarbonate
Celanese FORTRON MT9140L6 PPS, 40% Medical Technology
RTP Company RTP 2000 HC Polyester Alloy Medical Cleaner Resistant - UV Stabilized

PQZSA30514 / 178150

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.