MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® NX1440 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Dry as molded. Injection molding grade. Nylene NX1440 is a medium viscosity, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from NX1440 have better dimensional stability at moisture equilibrium than parts molded from conventional nylon. Nylene NX1440 provides for an excellent balance between stiffness and toughness. Optimum processing conditions should provide a melt temperature of 460 - 480ºF at the nozzle.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 1.5 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 75.0 MPaASTM D638
Elongation at Break 25 %ASTM D638
Flexural Yield Strength 114 MPaASTM D790
Flexural Modulus 2.90 GPaASTM D790
Izod Impact, Notched 0.400 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 245 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon
Nylene® PA6 Mineral Filled 6240 HS Nylon 6
Nylene® PA6 Impact Modified 421 HS Nylon 6

PN6C4X / 54231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.