MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lucite International Lucite® 30B Acrylic Resin for Dental Applications
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Lucite 30B is a designed for use in the manufacture of dental appliances. Lucite 30B resin contains residual initiator which allows this polymer to be processed using either dough molding or dry compression molding techniques. Lucite® 30B can be blended with methyl methacrylate resins to impart softness.
Lucite® 30B acrylic resins provides the benefits of improved flexibility and containing residual initiator.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.84 lb/gal
Water Absorption 0.29 %
Viscosity Measurement 0.41 - 0.45Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75
Tensile Strength 37.0 MPa
Elongation at Break 3.0 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.491
Transmission, Visible 92 %
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Colacryl® TS 1672 Acrylic Orthodontic Polymer
Lucite International Colacryl® PD12 Acrylic Dental Resin
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade
Lucite International Colacryl® DP300S Acrylic Dental Resin
Lucite International Colacryl® PD11SG Acrylic Dental Resin

PLUCIT9492 / 150206

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.